By aherna21
Date 04-16-2008 14:12
Edited 04-22-2008 12:36
_ POST Moved to general - Technical
Does anyone have experience with welding martensitic steels through electroslag welding? Is this recommendable?
ASME Boiler and pressure vessel code has a limitation for electroslag to be use donly on ferritic and austenitic steels,
Why does ASME code limit the use of ESW to ferritic and austenitic steels? (Section VII, Division 1, PART UW-5 (d))
Does this mean that ESW should not be used to weld marthensitic stainless steel?