- - By nagawade pratap Date 04-25-2008 13:09
kindly let us know the visual difference between welding by E6013 & E 7018 welding electrode
Parent - By js55 (*****) Date 04-25-2008 13:30
Not tryin got be a smartass here but why don't have your supplier give you some samples and see for yourself?
Parent - - By darren (***) Date 04-25-2008 16:58
do you already have existing unidentified rods and are trying to determine what rods you have by their appearance or bead appearance?
this seems an odd question.
perhaps more info on the reasoning for the question and more info besides just a name on your profile might help as well.
darren
Parent - - By 803056 (*****) Date 04-26-2008 18:11
With the number of questions posted by this visitor, it would appear he's having us help him with a homework assignment.

Al
Parent - By bozaktwo1 (***) Date 04-28-2008 16:56
Well, I certainly hope the dude passes.  Or maybe not.  I have a hard time with people who expect to cite a test question and simply receive the answer.