- By orlotron Date 05-13-2008 22:25
We do some brazing (induction and torch) for the Govt. We have a project that calls for torch brazing to AWS C3.4 (no class specified so we are assuming Class C). For the brazing alloy we're told to use Welding Rod per AWS A5.14 Type II, Class 5, .125" dia.
Problem - we can't cross over the Type and Class. Anyone know what the current equivalent material is?
Any experience with using this material for brazing? What Flux?
By the way - we're braze plain old 1018 C'steel.
Thanks in advance for any help or suggestions.
Steve