Can anyone tell me whether AWS D1.1 has incorporated ASTM A992 into it's documentation?
I'm still specifying ASTM A572 grade 50 steel with special requirements per AISC Technical Bulletin #3, March 1997. It's my understanding that it's inadvisable to spec. A992 until AWS has caught up.
If they have, I'll switch to specifying A992.