- - By mongoose Date 05-31-2008 14:30
What is the maximum allowable convexity in a fillet weld?
Parent - By jrw159 (*****) Date 05-31-2008 14:44
mongoose,
   Ass-u-me-ing you are working to D1.1 06 see section 5.24 through 5.24.3 and figure 5.4

jrw159
Parent - By Shahid Nazir Date 06-04-2008 16:58
Talking of fillet welds. What is the difference in fillet weld qualification between ASME and AWS.