could someone tell me about things i can do to trick it out has 750hrs on it has a good arc with hy/low rods. i think it could run 6010 better but not sure its hardly been used the guy i bought it from didnt know what he had got it for 1500 dollars
Get a Remote/Ditch box kit for it. Not the one that Lincoln sales. Get a Good one that has a power outlet on it for your grinder. Then do like Old School Pipe said and weld with it.