Up Topic Welding Industry / Technical Discussions / Welding for the fittings
- - By ravichk25 Date 06-25-2008 15:10
Can we weld a ellbow fitting to ellbow fitting directly??? What will be the consequences???
Parent - - By 3.1 Inspector Date 06-25-2008 15:12
Can we weld a ellbow fitting to ellbow fitting directly???......Yes.

What will be the consequences???....You just saved yourself a weld.
Parent - - By ravichk25 Date 06-25-2008 15:19
What I know wanted without using any pipe connected with ellbow can we weld directly with ellbow to ellbow?? Its operating at very high pressure at 270 bar?
Parent - By 3.1 Inspector Date 06-25-2008 15:22
To be honest, I dont see why not.
If you had high velocity, it might be an issue.