Every time I've seen (and worked with) tube to tubesheet welding, either in condensers and heat exchangers, the welding procedure specification was given by the equipment manufacturer. The erector (I suppose that you are the erector) has nothing to do but following those instructions.
Giovanni S. Crisi
Sao Paulo - Brazil