What is the best filler for welding pipe schedule 10 S-8 to S-8 (304 stainless) which will be used for cryogenic applications (liquified natural gas) @ -240 Deg F.
I have always used either 308 or 308L to weld 304, but I have seen 316L used for the describe application. Any advice would be greatly appreciated.