What code does one use when inspecting or welding on derricks in the oil field. I assume that and API code of some sort is being used. Does anyone know which one it is?
By
dbigkahunna
Date
07-26-2008 18:06
API RP 4G Recommended Practice for Use and Procedures for Inspection, Maintenance, and Repair of Drilling and Well Servicing Structures
By
doyenofcastle
Date
09-28-2008 16:55
4F may be used
Topic
Welding Industry
/
Inspection & Qualification
/ Derrick Inspection
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill