- - By BPI1 (*) Date 08-07-2008 00:05
Hey everyone!  I have a quick question, and I can't seem to find the answer.  I have a certification in vertical 3/8 plate w/ backing strip, 7018 filler.  I know that this lets me weld grooves in flat, horizontal and vertical positions, but what positions can I weld a fillet in?  Thanks for your help!
Parent - By swsweld (****) Date 08-07-2008 02:03
In D1.1 Table 4.10  Welder Qualification. If you test in the 3G position you can weld fillets in the F,H,V position. Same positions as the groove. You only get OH if you test in the 4G (or 4F for fillets)positions.

Of course taking a V and OH will give you all positions.