- - By Liz H Date 09-10-2008 19:30
We have been having issues with anodize not sticking to some of our aluminum braze parts.  The braze itself is coming out really dark in some cases, with flecks of anodize missing.  Any ideas as to what might be causing this?
Parent - By DaveBoyer (*****) Date 09-11-2008 04:18
Some filler materials just are not compatible with anodizing, has this process worked with this same brazing alloy in the past?