- - By afshin108124 Date 09-15-2008 10:48 Edited 09-15-2008 10:55
We considered (Fi)=1 for welds in designing the steel structure(for steel structure of steel complex company), is it intended that we should do 100% Radiography or Ultrasonic Test for CJP Butt welds?
I could not insert the symbol of (Fi),(Fi: weld efficiency)
Parent - By CWI555 (*****) Date 09-15-2008 12:34
What code? Joint type etc?