Up Topic Welding Industry / Technical Discussions / IPM settings on wire feeders
- - By Sean Landrum Date 09-29-2008 20:36
When the pre-qualification lists 10-12 ipm, does that mean x it buy 100 as it states on the wire feeder; making it 1000-1200 ipm?
Parent - By hogan (****) Date 09-29-2008 21:17
I think you might be confused about wire feed speed vs  inches per minute of weld deposited. Wire feed speed (wfs) is measuring how many inches of wire are coming out of the gun per minute. Hold the trigger for 10 seconds, measure the length and times that by 6, and that equals your wfs. Inches per minute is measuring the length of weld. This is done per minute of welding.
Parent - By kipman (***) Date 09-30-2008 12:23
Hogan's right.  You're looking at inches per minute of travel speed (deposited weld metal).
Mankenberg
Up Topic Welding Industry / Technical Discussions / IPM settings on wire feeders