- - By strat (**) Date 10-30-2008 12:01
could someone correct me if im wrong. A wt6 x 15 at 12' long for a vertical brace the permitted variation for camber in ASTM A6 is .125 x (number of feet of total lenght/5). that being im comeing up with 5/16" camber.Is that correct?
Parent - - By swnorris (****) Date 10-30-2008 13:32
Correct, unless AESS.
Parent - - By strat (**) Date 10-30-2008 15:26
thanks swnorris, but what is AESS
Parent - - By swnorris (****) Date 10-30-2008 15:29
Architecturally Exposed Structural Steel.  It's mainly cosmetics.  The straightness tolerances are one half of the camber and sweep tolerances in A6.
Parent - By strat (**) Date 10-30-2008 15:43
good deal, thanks swnorris