Thanks for the replies to my question. checked it out today. No smoke, oil looks good (as per your replies I assume), new mag, has all sheetmetal except sides and gas tank. also got 200 ft of 2/0 lead. Puts down a bead like a dream. For $1000 I can aford to put it back on gas.
also got paper work for the rebuild