D.1.1 section 4 doesn’t consider Combination of welding procedure contrary to ASME SEC. IX. Why?
QW-200.4 in ASME SEC. IX, is only about Combination of welding procedures. In accordance with QW-404.4, Filler metal F-Number, E6010 & E7018 have different F-Numbers; and according to QW-253 F-Number is an essential variable. Sometimes we use combination of E6010 & E7018 electrodes. Must we use QW-200.4 for this case?