I can not see anywhere in AWS D1.1, 2006 mentioned about Alternate Base Materials for Welder Qualification like ASME IX-2006, QW-423. Please inform me about this problem.
There is no problem. Base metal specification is not an essential variable for welder qualification in D1.1. Welder qualification must be performed in accordance with a WPS (which could be either prequalified or qualified), but a change in Group Number or to an unlisted base metal is not an essential variable for performance qualification.