johnnyh
Date
01-05-2009 19:18
Is it possible to use a Vantage 500 in a 300 frame?
By
JeremyW83
Date
01-05-2009 19:48
Yes, Cactus on here recently got one from the factory that way. They are special order I believe he said. He likes it from what I have heard.
By
Cactusthewelder
Date
01-05-2009 22:36
The 500 in a 300 frame is availible from lincoln. It is new this year
Topic
Welding Industry
/
General Welding Discussion
/ Vantage
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill