- - By keyholen (*) Date 02-15-2009 00:18
welding with 8010 3/16 i have not been able to make the bottom 4inches of 12inch pipe look any where as slick as the top and the sides any suggestions would be greatly appreciated
Parent - By dbigkahunna (****) Date 02-15-2009 16:14
If it is going flat, slow down/turn he heat down as you come up on the bottom. 10-15, not just 5
If it is humping up, speed up or turn up the heat.
My quess is it is going flat. It is really hard to determine what is wrong with out looking at a what you are doing.