Dear All,
I have a PQR already qualified on plate GMAW root / fill+capp FCAW, CJP.
I am covered to weld only FCAW fillet weld? Normally this is a combination of processes I need to keep, but what's the reason in case of fillet weld??
Please refer to art in AWS D1.1.