- By Nalla (***) Date 07-01-2009 23:44
Dear Friends
I've have 2 separate WPS/PQR-01 qualified using SMAW & FCAWx EH36 X EH36 x 25.4mm THK. plate with -40 Degree Celcius.Based on Table 4.6#2-Min. Thk qualified is 16mm . Is there anyway i can waive form this requirement and use  the same WPS/PQR-01 weld to DH36( -20 degree celicius ) material with 10mm thk? Weld Process either SMAW/FCAW.

Is there anywhere in the code allow such deviation

Appreciate any advise/guidance