General Welding Discussion
/ Branch Test
By
junkiron
Date
07-13-2009 05:00
What size wall is used for the branch test.
By
B.acosta
Date
07-13-2009 05:07
.250 or .375 wall
By
rondar
Date
07-13-2009 20:23
.375
By
B.acosta
Date
07-15-2009 03:28
i've tested on both
By
Shane Feder
Date
07-15-2009 03:45
If it is API 1104 it is .250 minimum (Clause 6.3.1)
Regards,
Shane
Topic
Welding Industry
/
General Welding Discussion
/ Branch Test
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill