- - By Gary Oakes Date 03-19-2002 20:42
I'm reviewing for the precast concrete industry our quality control manuals which reference an AWS table for the "minimum mechanical property requirements for studs" and would like to receive your most current version of this table. Please provide by e-mail or fax to 317-357-6012.

Thanks so much for the help.
Parent - By DGXL (***) Date 03-20-2002 02:36
The mechanical property requirements for studs can be found in AWS D1.1:2002, Table 7.1.