- - By Nalla (***) Date 08-01-2009 14:08
Dear Friends
I have 6GR PQR qualified to AWS D.1 with -40 CVN Value - Weld Process - SMAW
Question in ref to AWS D1.1 Table 4.5
1) Can I use it to weld Single V/Doube V / T-FP Single Bevel / Double Bevel Joints in 1G,2G,3G,4G & 1F,2F,3F,4F  using SMAW?
If can how about the welding parameters for various positions?
Any help appreciated
Parent - By 803056 (*****) Date 08-02-2009 15:57
You now have a qualified WPS that can be applied to other groove details including all of the prequalified joint details of D1.1 and complete joint penetration groove welds welded from one side without backing within the parameters of Clause 4, Table 4.5 for welds without notch toughness and Table 4.6 when the welds are required to meet notch toughness requirements.

Best regards - Al