TolgaKantaroglu
Date
03-21-2002 11:52
I am seeking for an EN standard for visual weld bead inspection. Does anyone know a spec. for visual inspection. Thanking you in advance.
Regards.
Tolga
By
TimGary
Date
03-21-2002 15:18
The American Welding Society (AWS) has published-
B1.11:2000 Guide for the Visual Examination of Welds.
I am not familiar with EN Standards.
By
TolgaKantaroglu
Date
11-02-2002 10:42
Thank you for your reply
By
adavis
Date
11-01-2002 21:16
EN 970
By
TolgaKantaroglu
Date
11-02-2002 10:41
Thank you for your reply
Topic
Welding Industry
/
Technical Discussions
/ Spec for Visual Inspection
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill