- - By miguel P (*) Date 03-26-2002 11:56
I would like to know why the juncture of welds in orthogonal directions shall be avoided? The weld access holes doesn´t must be closed for this reason.
Regards. MiguelP
Parent - By CHGuilford (****) Date 03-26-2002 14:27
You might want to take a look at the commentary to 5.17 from AWS D1.1. I think it will give you some useful information. Besides the difficulties in getting a full penetration weld at the web / flange juncture, weld cracking could be an issue without weld access holes.
Respectfully,
CHGuilford