- - By steelman7018 (*) Date 08-13-2009 19:33
ASME VIII vessel.  If the contract specifies PWHT then the WPS and PQR must indicate, correct?
Parent - By js55 (*****) Date 08-13-2009 19:40
The WPS must address PWHT if it is required. And there needs to be a PQR that supports the WPS for PWHT.