/ 13.8.2 Rejection Based on Strip Chart
By
DAYANARA
Date
10-05-2009 00:38
Dear All
Please help me, I not understand requirement in API 1104 - 13.8.2 Rejection Based on Strip Chart.
What's in meaning of Strip Chart?
Thank you for your aswer.
Dayanara
By
CWI555
Date
10-05-2009 02:11
13.8.2 is detailing what happens if the automatic welding strip chart (record of volts/amps/travel speed etc) deviates from the procedure specification.
If the strip chart does deviate, your required to remove the weld from the line.
Regards,
Gerald
Topic
Welding Industry
/
Technical Discussions
/ 13.8.2 Rejection Based on Strip Chart
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill