Hi
can you help me
Is the thickness of metal base a essencial variable for Welder Qualification under ASME IX, SMAW proceess
Thanks
By
jarcher
Date
10-20-2009 05:57
Yes. The thickness qualified for is 2t when the test is less than 1/2 thick. If it is 1/2" or greater and the welder makes 3 passes or more, the qualification is to the thickness limits of the WPS.
By
robin toscano
Date
10-21-2009 12:22
What about the minimum qualified thickness ? Where is that in code ?
thanks
By
RonG
Date
10-21-2009 13:02
Edited
10-21-2009 13:28
Try table QW-450 for PQR & QW-452.1 Weldor qualification.
Topic
Welding Industry
/
Technical Discussions
/ Werder Qualification under ASME IX
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill