In table 4.11 of AWS D1.1 under fillet weld option 2 is the reference to Fig 4.32 a typo? Should it be Fig. 4.33?
Jim Hughes
By
803056
Date
10-27-2009 22:27
I don't have my 2008 edition, but did you check for errata on the AWS website? That should list all the errata found to date.
Best regards - Al
By
waccobird
Date
10-28-2009 11:57
Maybe My AWS D1.1 2008 In table 4.11 under fillet weld option 2 is the reference Fig. 4.33
So if yours has 4.32 I guess it is a typo in your book.
Hope this helps more than hurts
By
Jim Hughes
Date
10-29-2009 00:10
waccobird,
Thanks. That helps a bunch.
Jim Hughes
Topic
Welding Industry
/
Inspection & Qualification
/ Fillet weld test
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill