Hello,
We have WPS/PQR qualified for P No.1 Gr1 can we weld the material P No.1 Gr 2 .
Thank you
Dhanna
By
js55
Date
11-10-2009 13:34
Yes. As long as impacts aren't imposed.
By
jon20013
Date
11-11-2009 02:04
and even when impacts are imposed, there's some slippery language in the variable that would allow you to make an engineering judgement if there's any effect.
Topic
Welding Industry
/
Technical Discussions
/ WPS/PQR Base Material for Procedure Qualification ( QW 424)
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill