- - By Metarinka (****) Date 11-13-2009 18:46
does AWS have any specifications in the filler material codes that deal with wire cast and helix?

I think I got a bad batch of wire, but for future reference it would be nice to know the cast and helix requirements if there are such a thing.

Wire is  ER80S-2
Parent - By 803056 (*****) Date 11-13-2009 20:03
Look in the applicable filler metal specification or A5.01. One or the other will have it.

Best regards - Al
Parent - - By kipman (***) Date 11-13-2009 20:46
Joel,
You're looking for A5.28 Clause 18.
Mankenberg
Parent - - By Metarinka (****) Date 11-13-2009 21:33
sounds good, unfortunately I don't have access to A5.28, unless it's one of the supplemental references AWS gives out for free?