- - By Todd Bitter (*) Date 05-30-2002 14:22
I can not seem to find any info on this material. Has anyone heard of this material? I know it is for high temp service and I believe it's a nickel alloy of some sort. I have checked ASTM, ASME and can not find it. Thanks for the help.
Parent - - By GRoberts (***) Date 05-30-2002 14:44
Try this link. The RA in RA330 is for the company Rolled Alloys.

http://www.rolledalloys.com/mainentry/index.asp
Parent - By Todd Bitter (*) Date 05-30-2002 14:54
Thank you very much!