Not logged inAmerican Welding Society Forum
Forum AWS Website Help Search Login
Up Topic Welding Industry / Technical Discussions / AWS D1.1:2002 2.18
- - By TimGary (****) Date 06-19-2002 15:04
AWS D1.1:2002 2.18 Inspection states:

"Fatigue categories B and C require that the Engineer ensure that CJP groove welds subject to cyclic transverse applied stress into the tensile range be inspected using RT or UT."

Could someone please define "categories B and C" in relation to a typical Metal Building System?

Thanks in advance for your time,
Tim Gary
Parent - By Wildturkey (**) Date 06-19-2002 16:19
Tim I think table 2.4 starting on page 25 will help with what you are looking for....I hope this helps
Up Topic Welding Industry / Technical Discussions / AWS D1.1:2002 2.18

Powered by mwForum 2.29.2 © 1999-2013 Markus Wichitill