Welding Industry
/
General Welding Discussion
/ Semi Auto Arc Gouging
By
Steve.E
Date
03-11-2010 03:16
Hi guys , can anybody give me a contact or link for a Semi Automatic Arc Gouging Head manufacturer.
By
PhilThomas
Date
03-14-2010 14:16
Arcair makes a mechanized carbon arc rig:
http://www.thermadyne.com/IM_Uploads/DocLib_739_89-240-004.pdf
HTH
By
Steve.E
Date
03-16-2010 10:17
Thanks for the link Phil, we have one of those auto units, but I'm chasing a semi auto unit, box shape head with wheel you turn by hand to feed carbon rod through.
Topic
Welding Industry
/
General Welding Discussion
/ Semi Auto Arc Gouging
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill