Up Topic Welding Industry / Technical Discussions / Spot Welding, Stainless Steel
- - By Engineer Ray Date 07-26-2002 16:31
What specifications covers the topic of Spot Welding, Stainless Steel?
What I am looking specifically for testing methods for checking the spot welds in stainless steel, both non-destructive and destructive.

Thank you in advance for your time and help.
If you would like to discuss this with me let me know and I will give you my phone number.

Best Regards,
Ray
Parent - By DGXL (***) Date 07-27-2002 02:46
Pull, peel, tensile and macroetch testing?
Parent - By qualls Date 07-27-2002 15:28
The information you are seeking can be found in the bulletins presented by the AWS 'C-1' committee. Low carbon steels and stainless steels fall under the same categories for destructive testing. See Bulletin "C4"