does anybody know something about dissimitar metal welds between magnesium and other metals (e.g. aluminium...)? Does there exist projects about this topic?
TWI has every month a free weldasearch on different subjects on there site. I just saw the current search on joining magnesium. Maybe you can find an answer there.