Curious on everyones opinion about having an xray inspection on a .250" fillet weld. Flange (1.80" THK) to pipe (.750 SCH 80). This will be a dual pass weld, unsure if their is any value in being xrayed since it is fillet welded.

I have heard that it is tough to determine weld imperfections through xray when they are fillet? Anu opinions? Or if possible a third party xray provider in Central Texas?