/ Lean Duplex: ASME P number
By
Dave Dove
Date
08-09-2010 06:57
I am trying to find the ASME P number for S32010/ S32304 lean duplex grades, in order to us on Air Coolers etc.
Any assistance wouls be appreciated.
Regards Dave
By
pipewelder_1999
Date
08-09-2010 11:03
Go to pnumbers.com
Gerald Austin
Topic
Welding Industry
/
Technical Discussions
/ Lean Duplex: ASME P number
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill