thanks.
wire speed 180-280 ipm
horizontal position,downhand
19.5-22v
tri-mix 90% helium, 7.5% Argon and 2.5% co2
short circut
manual
The weld shape is crowned up on downhill welds, but humped in horizontals, edges seem undercut but weld contour is humped.
Just having trouble getting a pretty weld! Weld color is there front and back w/ no sugar. Just doesn't look like I think it should.