- - By TERRYFSDG Date 09-10-2002 18:55
I am looking for any and all code specifications on spot welding stainless and carbon steels. can someone send me this at terry.l.howard@power.alstom.com
thank you
Parent - - By chapple (*) Date 09-11-2002 17:35
Terry,

If it would be of any help to you I can send you automotive spot weld
specifications, both domestic, and foreign.

Parent - - By TERRYFSDG Date 09-11-2002 18:07
That would be extremely helpful, my email adress is terry.l.howard@power.alstom.com or you can fax it to 860-285-4020
attn: Terry Howard FSDG
thank you,
Terry
Parent - By DGXL (***) Date 09-13-2002 03:53
Get your hands on a copy of the AWS Welding Handbook - Volume 1 (Welding Technology - 8th Edition), there is everything you'll need reference-wise pertaining to RSW.
Parent - By noswal Date 11-12-2002 16:44
Scott Chapple.,If you could be as kind to send me the same, I would be much apprecative. Thanks

Nos
Parent - By rhoople (*) Date 10-08-2002 20:34
Better yet, get your hands on the AWS C1.1, Recommended Practices for Resistance Welding.