Not logged inAmerican Welding Society Forum
Hello my friends
i wanna weld two similar stainless steel (304 or 316L) and simulate the intergranular corrosion due to sensitization and chrome depletion with fluent (or abaqus)
please introduce some related article
respectfully . Mohsen
You forgot to state the electrode, MIG wire or TIG rod you're going to use.
Giovanni S. Crisi
Sao Paulo - Brazil
What filler rod are you going to use on this.
M.G.
Moshen,
See ASTM A262, Standard Practices for Detecting Susceptibility to Intrgranular Attack in Austenitic Stainless Steel.
Hector Garcia
sorry i forget to explain , the welding method is TIG and the filler is Y308L probability , i now just want some article for history background and if you had the same experiments please guide me .
thank my friends...
Powered by mwForum 2.29.2 © 1999-2013 Markus Wichitill