- - By Blaster (***) Date 10-30-2010 19:50
Euro (Dinse) style or Tweco style lead connector?

Which do you primarly use and why?
Parent - By TRC (***) Date 10-30-2010 23:47
I use Dinse. Never had one fail. I do recall Tweco spinning and not making a good connection.  I have had a few for many years, they take a lickin and keep on tickin.
- - By Sberry (***) Date 10-30-2010 20:57
Tweco, started with them, very common.
Parent - By Cactusthewelder (*****) Date 10-30-2010 21:01
Tweco LC-40. Most common out there
- By Sberry (***) Date 10-30-2010 23:03
Cant recall ever running across anything else on a job.
- By scrappywelds (***) Date 10-31-2010 01:04
tweco all the way. if u do run into something esle just make an adapter for it.