- - By jsdwelder (***) Date 02-08-2011 16:29
Does anyone know what certifications Massachusettes requires for welders to weld on bridges in that state?
Parent - By 803056 (*****) Date 02-08-2011 18:06
I believe they require the welder to test to D1.5.

Best regards - Al
Parent - By psnort (*) Date 02-08-2011 22:47
Mass Highways - They have you go to a testing center and test to D1.5. They issue you a card that they have to sign off on every 6 months and a certificate with your picture. 3 & 4 G, 3/8" limited or 1" unlimited. Call ABC Testing in Bridgewater or Triangle in Hanover for more info.
- By jsdwelder (***) Date 02-09-2011 19:27
Thanks guys