- - By Blaster (***) Date 02-08-2011 21:59
What is the name and the numeric designation for the AWS publication that defines standard welding terms?

Thanks
Parent - - By waccobird (****) Date 02-08-2011 22:18
Blaster
AWS A3.0M/A3.0:2010
      
Standard Welding Terms and Definitions Including Terms for Adhesive Bonding, Brazing, Soldering, Thermal Cutting, and Thermal Spraying ?

Good Luck
Marshall
Parent - - By jrw159 (*****) Date 02-08-2011 22:22
Your quick! LOL :-)

jrw159
Parent - - By waccobird (****) Date 02-08-2011 23:21
John

Not really.
Now you want to talk about quick jwright650 is quick.

Marshall
Parent - By jrw159 (*****) Date 02-08-2011 23:49
He is quick too, but you hit the center ring before either of us cleared leather. :-)

jrw159
Parent - - By jrw159 (*****) Date 02-08-2011 22:21
AWS A3.0M/A3.0 Standard Welding Terms and Deļ¬nitions.

jrw159
Parent - By Blaster (***) Date 02-08-2011 22:35
Thank you guys, much appreciation!