- - By bamaCWI (**) Date 02-13-2011 15:58
Hello everyone. I have a requirement to qualify a WPS for Inconel 625 to Inconel 713 using ER NiCrMo-3 filler, manual GTAW. I am not familiar with the 713 but from what information I have found, it appears to only be available in casting. I am looking for any information, tips, and/or experiences with this combination of materials.
Thanks
scott
Parent - By G.S.Crisi (****) Date 02-14-2011 17:55
Any Inco catalog will tell you that. If you havn't one at hand, ask Inco:
www.inco.com
Giovanni S. Crisi
Sao Paulo - Brazil
Parent - By ssbn727 (*****) Date 02-19-2011 07:20
Here is a good link or two that will help you find what you're looking for:

http://specialmetalswelding.com/

http://www.specialmetals.com/contact.php

Here is an interesting thread from another forum regarding the weldability of Inconel 713 FWIW...

http://www.eng-tips.com/viewthread.cfm?qid=158984&page=120

It appears that the 713 is not as readily weldable as the 625 is, and as Professor Crisi suggests - contacting Special Metals via the second link shown above is probably the best course to follow in order to get the knowledge you need regarding your query.