for AWS 5.01 and 5.1 the difference between test schedule F and I is that : table 2 tests will be in A test  report  for I schedule but for F schedule is not required test report .Am I right ??
last time I received test report for 7018 4mm dia. there is no x-ray results in the report ,I asked for that the supplier said schedule F not required to be add to the report only chemical and impact and tension results , I didn't argued with him because when I looked at the 5.1 I didn't interpreted clearly the words .any one can help