- - By eekpod (****) Date 02-23-2011 22:38
Everyone,
A few months back someone had posted an article that discussed bend test results and situations to look for and had illustrations of different reasons why face and root bend test failed.

I saved it becasue it was a good article, problem is I don't know where I saved it (both hard copy and electronic).

Anyone remember this? please attach if you have it,
Thanks
Parent - - By jwright650 (*****) Date 02-24-2011 12:16
Parent - By eekpod (****) Date 02-25-2011 11:26
Yes!! Thanks John that's the one.