hello dear friends
during TIG welding of a240 gr.316 to a387 gr.11, we can do both argon purging and back weld for achieve to sound root pass. I want to know which case is appropriate in relation to mechanical properties of weld? is there posobility of weld cracking with back weld?
thanks for your mention